Fiber mist eliminators in chlor-alkali: three positions, one material trap

Acid mist elimination in a WSA plant: the square ETFE element and the tube-end mesh roll
11/26/2026
CFD velocity magnitude in a double-pocket vane channel at 5 m/s, showing 5 to 8 m/s in the core and 1 to 2 m/s in the pocket
Double-pocket vane packs: reading the CFD, and what it cannot prove
11/27/2026
Acid mist elimination in a WSA plant: the square ETFE element and the tube-end mesh roll
11/26/2026
CFD velocity magnitude in a double-pocket vane channel at 5 m/s, showing 5 to 8 m/s in the core and 1 to 2 m/s in the pocket
Double-pocket vane packs: reading the CFD, and what it cannot prove
11/27/2026
Key facts

  • A chlor-alkali plant needs a fiber bed in three different places, and each one is there for a different droplet size: brine fog at the cell outlet, sulfuric acid mist at the drying tower exit, and carryover ahead of the chlorine compressor.
  • The drying-tower mist that matters is 0.3 to 1 µm. A knitted mesh pad, which cuts at roughly 10 µm, is not a cheaper version of a fiber bed in this duty; it is a different device that does not see the droplets.
  • Fiber beds are sized on media velocity, 0.2 to 0.5 m/s, not on vessel cross-section, and they cost 0.5 to 2 kPa of pressure drop that the chlorine compressor pays for every hour of the year.
  • The outlet guarantee in chlorine drying is normally written as below 20 mg/m³ at design flow, and that number is set by the compressor and the liquefaction train, not by the tower.
  • The material decision is decided by water content, not by chlorine: titanium is passive in wet chlorine and a fire risk in dry chlorine, which is why the same plant uses titanium before the drying towers and C276 or PTFE-lined steel after them.

Where fiber beds sit in a chlor-alkali plant

“Fiber mist eliminator” is used loosely in chlor-alkali, and that looseness causes most of the wrong specifications. There are three positions, three duties, and only two of them are genuinely fiber-bed duties.

Position What is in the gas Droplet size What belongs there
Cell gas outlet / chlorine cooler Brine fog, NaCl aerosol, traces of caustic carried as spray Mostly 3 to 50 µm, with a fine tail Mesh pad or vane pack, plus a wash if the fine tail matters
Drying tower exit (concentrated H2SO4) Sulfuric acid mist, plus SO3 that condenses on the way out 0.3 to 1 µm Fiber bed, no substitute
Compressor suction or discharge, liquefaction tail gas Acid carryover from the towers, fine aerosol from the compressor Sub-micron Fiber bed, or a scrubber followed by a fiber bed

The pattern is the same one that runs through every mist-elimination decision on this site: the device is chosen by the droplet size the duty actually produces, not by the name of the equipment package it arrives in. A mesh pad placed where the mist is 0.5 µm will look like it is working — it will be dry, it will have a sensible pressure drop — while passing almost everything through.

Why a mesh pad does not close this gap

A knitted mesh pad removes droplets by interception and impaction: the droplet has enough inertia to leave the gas streamline and hit a filament. Inertia scales with droplet mass, so the mechanism dies quickly below about 10 µm and is essentially absent at 0.5 µm. At that size the droplet follows the gas around the filament as if the filament were not there.

A fiber bed works on a different mechanism. The fibers are two orders of magnitude finer than mesh filaments, the gas velocity through the media is low, and the residence time inside the media is long. At 0.3 to 1 µm the dominant capture mechanism is Brownian diffusion: the droplet is small enough to be buffeted by gas molecules and to wander onto a fiber rather than to be thrown at it. Diffusion capture improves as velocity falls, which is exactly the opposite of the mesh pad, and that is why fiber beds are sized on a low media velocity rather than pushed to a high face velocity to save steel.

The trade is pressure drop and space. A mesh pad costs 0.05 to 0.3 kPa; a fiber bed costs 0.5 to 2 kPa, and it needs a housing, a support grid and a sealing arrangement that a pad does not. There is no version of this where a mesh pad is the cheap answer to a sub-micron duty.

The drying tower is where most of the mist is born

Chlorine leaves a membrane cell hot and water-saturated — around 80 to 90 °C, with water vapour making up tens of percent of the gas volume. It is cooled and washed before drying, and the drying itself is done counter-current with concentrated sulfuric acid: typically 96 to 98% acid at the top of the last tower, diluted as it travels down and returned to the acid loop for reconcentration.

The mist at the tower exit has three sources, and they behave differently:

  • Carryover from the tower packing. Acid flung off the packing as the gas turns. These droplets are the largest ones in the stream, often 5 to 20 µm, and they are the reason some plants get away with a mesh pad for a while before the guarantee is tightened.
  • Condensation in the gas space and the outlet duct. The gas leaves saturated with sulfuric acid vapour at tower temperature and cools a few degrees in the duct. Vapour condenses as a fine fume, 0.3 to 1 µm, which no inertial device can catch.
  • SO3 carried through the tower. Any SO3 that survives the drying tower forms sulfuric acid aerosol downstream. It is the finest and the most corrosive fraction, and it is the reason the outlet limit is written as 20 mg/m³ rather than in droplet size.

The consequence for specification is direct: if the plant is buying a fiber bed on the strength of a mesh-pad experience, the guarantee it writes will be met on commissioning and missed two years later, when the condensation fraction has grown because the tower is running hotter or the acid strength has drifted.

Sizing on media velocity, not on face area

Fiber beds are not sized like a mesh pad, where the vessel area times a K value gives the capacity. They are sized on the velocity through the media and on the media area required to hold that velocity, with the housing sized around the resulting candle array.

Design media velocity in chlorine drying service is usually quoted between 0.2 and 0.5 m/s, lower where the outlet limit is tight or the aerosol is very fine, higher where the media area has to fit an existing housing. Two numbers set the choice:

  • Efficiency at the cut size. A fiber bed is commonly specified at 95 to 99.9% on 0.5 µm, and the number falls off below 0.1 µm. Asking for 99.9% at 0.2 µm is asking for more media, more pressure drop, or both.
  • Pressure drop at the design flow. Clean media in this duty sits at the bottom of the 0.5 to 2 kPa band; the top of the band is what you see when the element is loaded, and it is the number that should be used for compressor sizing.

The pressure drop is not free, and the arithmetic is worth doing before the element is chosen. A chlorine stream of 20,000 m³/h across 2 kPa absorbs about 11 kW of ideal compression work; at a realistic 70% efficiency it is roughly 16 kW, which over 8,000 hours is about 127 MWh — a five-figure electricity bill in most of Europe or China, every year, for a device whose only job is to catch a few milligrams per cubic metre. A 0.6 kPa element and a 2 kPa element both meet a loose outlet limit; only one of them is cheap to operate.

Two practical consequences follow. First, the DP taps belong in the specification: an element without a differential pressure reading cannot be judged, and “it still works” is what a blinded candle looks like from the control room. Second, the housing has to be designed for the element that will actually be fitted, not for the element that was fitted in 1998 — the replacement candle is usually the point where the media area quietly shrinks.

The material trap: wet chlorine and dry chlorine

Chlorine is one of the few services where the same plant legitimately uses two different alloys on either side of the drying towers, and where choosing one alloy throughout creates a hazard rather than a saving.

Wet chlorine passivates titanium. With water present above roughly 1.5 to 2% by weight, a protective film forms and titanium behaves well — this is why cell gas lines, coolers and wet-side piping are titanium.

Dry chlorine does not. Below that water content, titanium can react with dry chlorine and is a known ignition and fire risk. The dry side of a chlor-alkali plant — after the drying towers — is therefore built in carbon steel, PTFE-lined steel, or nickel alloys such as C276, depending on the acid load and the temperature.

For the fiber bed itself, the materials that see service are:

Part Wet side (before drying) Dry side (after drying)
Media Glass fiber with PTFE binder, PVDF where fluoride attack is possible Glass fiber with PTFE binder; the acid mist is the constraint, not the chlorine
Housing and grid Titanium, PTFE-lined steel, or PVDF for smaller units Carbon steel with PTFE lining, C276, or 316L only if the acid is never dilute
Sealing and gaskets PTFE or PVDF; no elastomer that chlorine attacks PTFE, expanded PTFE, or acid-resistant elastomer with a PTFE facing

One trap deserves its own line: 316L is the default alloy in most of the process industry, and it is the wrong default on the wet side of a chlorine plant. Moist chlorine with even small amounts of condensation produces hypochlorous acid and chloride, and 316L pits. The fiber bed is usually the last place a pinhole leak is noticed, because it sits inside a housing that nobody opens until the DP tells them to.

How these elements fail in service

In chlor-alkali service the failures are rarely the dramatic ones. They are slow, and they show up as a guarantee that is missed by a factor of two rather than a candle that falls apart.

  • Blinding by dilute acid. Water carryover from upstream, or a tower upset that pushes weak acid through, wets the media and leaves a salt-and-acid film after the next drying cycle. The media does not recover, and the DP climbs permanently.
  • Gasket bypass. The candle seals against the tube sheet with a gasket or a clamped collar. A degraded gasket lets a fraction of the gas go around the media instead of through it: efficiency falls, DP falls with it, and the plant reads the lower DP as an improvement.
  • Fiber migration. Glass fiber that has lost its binder can migrate downstream. In chlorine service the downstream is a compressor or a liquefaction train, and fiber finds bearings and seals.
  • Support grid and housing corrosion. A grid that was specified for the commissioning acid strength, and then sees dilute acid during an upset, corrodes and sags; a sagging grid unloads the candles and opens a path around them.
  • Mechanical damage at handling. Candles are fragile, they are long, and they are usually changed by two people on scaffolding. A candle that has been dropped still looks intact from the outside and leaks from a cracked media bed.

Each of these has a signature, and the signature is the reason the DP tap and the outlet analyser have to be read together. A high DP with a good outlet is loading; a high DP with a bad outlet is blinding plus bypass; a low DP with a bad outlet is bypass.

What to measure before ordering a replacement candle

Aftermarket candles are a legitimate way to replace an OEM element, and the ones that fail are almost never the ones with a wrong fiber — they are the ones ordered from a drawing package that did not describe the housing. Before a quotation is worth reading, these eight numbers have to exist:

  1. Housing internal diameter and the tube-sheet or grid geometry the candle seals against.
  2. Candle outside diameter, length, and the media area that the original element actually had — not the area the catalogue claims.
  3. Sealing method: gasket type, collar, clamp, or bayonet, and the material the seal sees.
  4. Design flow and the flow at which the outlet limit must still be met.
  5. Design and maximum pressure drop, and where the taps are located.
  6. Acid strength range, including the dilute excursions during upsets.
  7. Water content and temperature at the element, because it decides both material and blinding risk.
  8. Outlet limit, with the method by which it will be measured.

The single most common error in this list is area. A replacement candle that fits the housing and seals correctly, but carries 20% less media area, will pass the acceptance test at the design flow and fail at the turndown or at the next campaign. Area is the number that has to be written into the purchase order, not inferred from the OD.

How this differs from a sulfuric acid plant element

The mechanical hardware is close to the same, and the duty is not. In a sulfuric acid plant the fiber bed usually sits on the absorbing tower exit, sees a stronger and hotter acid mist, and is sized against a very tight outlet limit with a large media area. In chlor-alkali the element sits after the drying towers, sees a smaller gas flow per unit area, and is constrained by a compressor that cannot afford pressure drop. The two services share a supplier base and a media technology; they do not share a specification.

That matters when a plant buys a candle on the basis of a sister site’s experience. The same factory, the same fiber, the same OD, and a different media area, because the gas flow and the allowable DP are different.

Frequently asked questions

Can a mesh pad replace a fiber bed in chlorine drying?

No. The mist is 0.3 to 1 µm and a mesh pad’s capture mechanism has effectively stopped working below about 10 µm. A mesh pad will run dry, show a low pressure drop, and pass the acid mist through.

What outlet acid mist can be guaranteed?

Guarantees are written as below 20 mg/m³ at the design flow, with the measurement method named. The number is usually set by the downstream compressor and the liquefaction train rather than by the drying tower itself.

Why does the pressure drop climb and never come back down?

Because the media has been wetted by dilute acid or by water carryover, and the resulting film does not re-dry cleanly. A fiber bed is not a washable filter in this service; the recovery is a replacement, which is why the water side of the tower is the thing to fix first.

Is titanium the right material for the element housing?

Only on the wet side. Titanium is passive in wet chlorine and a fire risk in dry chlorine, so a housing downstream of the drying towers should be carbon steel with a PTFE lining, C276, or an equivalent — not titanium.

How often should the candles be replaced?

On condition, not on a calendar: DP at the design flow, outlet acid mist, and a physical inspection of the seals. Typical media life in clean chlorine drying service runs several years; a plant that blinds them in a single campaign has a tower problem, not a candle problem.

Fiber beds in chlorine gas drying, fiberbed candle replacement in sulfuric acid plants, fiberbed versus wire mesh, material selection, what pressure drop to expect, the selection map by duty.